Most people never think about the nozzle until a print goes wrong. It is a small metal cone, cheap to replace, and it is the only part of the printer that actually touches the plastic. That makes it the part that wears, and the part whose wear is hardest to see.
Why brass is the default
Brass conducts heat well and is easy to machine, which makes it cheap and makes it heat the filament quickly and evenly. For PLA, PETG, ABS and TPU it does everything you need, and for most printing it is the right choice, not a compromise.
Its weakness is that it is soft.
What soft costs you
Some filaments are not just plastic. Carbon-fibre, glass-fibre, metal-filled and glow-in-the-dark materials all carry hard particles, and pushed through a nozzle at speed those particles act like a fine abrasive. Brass loses that contest. The hole at the tip slowly widens.
Nothing announces it. There is no error, no warning, and the printer carries on extruding exactly as instructed. But a wider hole lays down a wider line than the slicer planned for, so walls come out thicker, holes come out smaller, and fine detail softens. It is the same family of trouble as the one in the dimensional accuracy post, a printed number drifting from the designed one, except that this cause is invisible to every setting in the slicer. The software believes the nozzle is the size it was when you installed it.
What hardened steel changes
Hardened steel resists that abrasion far better, so the hole stays the size it was meant to be for much longer. That is the whole reason to use it.
It has costs. Steel conducts heat less well than brass, so the plastic at the tip can be cooler than the temperature the printer reports. In practice that often means a slightly higher temperature, or slightly slower flow, to get the same result you had with brass. It is also not a licence to ignore wear. Hardened steel wears more slowly, not never, and abrasive filaments will still get to it in the end.
Which to use
- Only standard filaments: brass. Hardened steel gives you nothing here and costs you some thermal performance.
- Occasional fibre-filled or metal-filled jobs: use a hardened steel nozzle for those jobs and go back to brass afterwards.
- Regularly abrasive materials: hardened steel as standard, and keep an eye on it anyway.
- Very small nozzles: be more careful with either metal, because the same amount of wear is a much larger fraction of a small hole.
How to tell a nozzle has worn
The signs are easy to misread as something else: under-extrusion that cleaning does not cure, walls consistently thicker than expected, detail that was crisp and no longer is. The most reliable check is the one from the earlier calibration post. Keep a coupon from when the nozzle was new, print the same coupon now, and measure both the same way. If the numbers have moved and nothing else has changed, the nozzle has moved them.
It also helps to count wear by what went through the nozzle, not by how long it has been fitted. A few spools of an abrasive filament will do more damage than a year of PLA.
A consumable that is also an instrument
Most of a printer's precision is built into the machine and stays there. The nozzle is the exception, a part of the measuring system that is allowed to wear out while everything around it stays the same. A printer is only ever as consistent as its smallest and cheapest component, and that is the one worth checking.